Although the quality of enameled wire depends to a large extent on the quality of raw materials such as paint and wires and the objective conditions of machinery and equipment, if the operation does not take a series of problems such as baking, annealing, speed, etc. seriously and understand their interrelationships , Without mastering the operating technology, not doing the touring work and parking finishing work seriously, and not doing well in the process and hygiene, even if the objective conditions are good, it will not be able to produce high-quality enameled wire. Therefore, the decisive factor for a good enameled wire is people, and people’s sense of responsibility for work.

Rated 4.8/5 based on 500 customer reviews
Share:
Content

1. Before starting the catalytic combustion hot air circulation enameling machine, the fan should be turned on to make the air in the furnace circulate at a slow speed. The furnace and the catalytic zone are preheated with electric heating, so that the temperature of the catalytic zone reaches the specified catalyst light-off temperature.

2. “Sanqin” and “Sancha” in production operations.
1) Dirty paint film: Measure once every hour, and the zero position of the micrometer is corrected before the measurement. When measuring the line, the micrometer and the line keep the same speed, and the big line should be measured in two mutually perpendicular directions.
2) Frequent school wiring ¡¡ Always observe the back and forth wiring and tension tightness, and correct it in time. Check whether the lubricating oil is proper.
3) Look at the surface frequently: frequently observe whether the enameled wire has graininess or paint peeling during the coating process, find out the cause, and correct it immediately. For the defective products on the car, unscrew the axle in time.
4) Check operation: Check whether the running parts are normal, pay attention to the tightness of the pay-off shaft to prevent rolling head, wire breakage and wire diameter thinning.
5) Check three degrees: Check temperature, speed and viscosity according to process requirements.
6) Check the raw materials: continue to pay attention to whether the raw materials meet the technical requirements during the production process.

3. In the enameled wire production operation, attention should also be paid to explosion and fire problems. There are several kinds of fire situations:
One is that the entire furnace is completely burnt, which is often caused by the excessive vapor density of the furnace cross section or the furnace temperature; the second is that the amount of paint on a few wires is too much when threading, which causes a few wires to catch fire. To prevent fire, firstly, strictly control the temperature of the process furnace, and secondly, make the furnace ventilated smoothly.

4. Finishing after parking
The finishing work after parking mainly refers to cleaning the old glue at the furnace mouth, cleaning the paint tank and guide wheel, and doing a good job in the enameling machine and the surrounding environmental sanitation work. In order to keep the paint tank clean, if you do not drive immediately, you should cover the paint tank with paper to avoid the introduction of impurities.